vol.24 número3Influencia del modo de grabado y del tipo de resina en la resistencia adhesiva al Biodentine utilizando un adhesivo universal tipo "no-wait"Efecto del modo y tiempo de fotocurado de la lámpara LCU Led de tercera generación en las propiedades mecánicas de los nanocompuestos índice de autoresíndice de materiabúsqueda de artículos
Home Pagelista alfabética de revistas  

Servicios Personalizados

Revista

Articulo

Indicadores

Links relacionados

  • No hay articulos similaresSimilares en SciELO

Compartir


Odovtos International Journal of Dental Sciences

versión On-line ISSN 2215-3411versión impresa ISSN 1659-1046

Resumen

JIMENEZ-HERNANDEZ, Melissa et al. Evaluation of dentin microroughness and composite bond strength after multiple uses of diamond burs. Odovtos [online]. 2022, vol.24, n.3, pp.48-60. ISSN 2215-3411.  http://dx.doi.org/10.15517/ijds.2022.49286.

Using a bur multiple times to prepare dental structure may produce a smoother final surface on dentin than a new one. This superficial roughness may affect adhesion with resin-based materials by modifying the substrates' characteristics. The aim of this study was to evaluate the effect of multiple uses of diamond burs on dentin's superficial microroughness and bond strength with resin composite when using a self-etch adhesive. Diamond dental burs were used to simulate a preparation (dentin flat surface) on extracted third molars. Samples were distributed into groups according to burs' number of previous uses as follows: 0, 1, 5 and 10. Scanning electron microscopy images at 70x, 350x, and 1000x were used to illustrate burs' deformation. Each specimen's dentin microroughness was measured three times to compare between experimental groups and the micro-shear bond strength test (n=15) was performed for the 0 and 10 uses groups using a universal adhesive in a self- etching mode. Diamond crystals wear and dislodgements were evident among groups where the burs were used more times. As the number of uses increased the mean microroughness of the dentin surface decreased with significant differences between the 0 and 10 uses groups. No statistical differences between experimental groups resulted from bond strength tests. When using a universal adhesive in a self-etching mode, the number of previous uses of a diamond bur seems to have no significant effect on dentin/resin composite bond strength.

Palabras clave : Adhesion; Bond strength; Dental burs; Microroughness; Multiple uses; Micro-shear.

        · resumen en Español     · texto en Inglés     · Inglés ( pdf )